韧性良好PA6 日本宇部 1013NW8中粘度 高流动 阻燃V-2
2024-07-25
产品详情
- 价格:21.5
- 产品名称韧性良好PA6 日本宇部 1013NW8中粘度 高流动 阻燃V-2
查看相似产品 >
- 简介
1013NW8
聚已内酰胺#尼龙6|PA6
泰国宇部
物性信息:
基本性能
|
额定值
|
单位
|
测试方法
|
吸水率
|
10.7
|
%
|
ASTM D-570
|
成型收缩率
|
1.3
|
%
|
UBEmethod
|
吸水率
|
1.8
|
%
|
ASTM D-570
|
成型收缩率
|
1.2
|
%
|
UBEmethod
|
物理性能
|
额定值
|
单位
|
测试方法
|
比重
|
1.14
|
|
ASTM D-792
|
机械性能
|
额定值
|
单位
|
测试方法
|
硬度(洛氏.布氏) (23°)
|
120
|
|
ASTM D-785
|
弯曲强度 (-30°)
|
1400
|
kgf/cm
|
ASTM D-790
|
挤剪强度 (23°)
|
650
|
kgf/cm
|
ASTM D-732
|
1%变形下的压缩强度 (23°)
|
100
|
kgf/cm
|
ASTM D-695
|
挤剪强度 (23°)
|
600
|
kgf/cm
|
ASTM D-732
|
弯曲强度 (23°)
|
400
|
kgf/cm
|
ASTM D-790
|
Taber磨耗率
|
7
|
mg
|
ASTM D-1044
|
抗冲击强度 (23°)
|
50
|
kgf.cm/cm
|
ASTM D-256
|
断裂下的伸张强度 (23°)
|
650
|
kgf/cm
|
ASTM D-638
|
弯曲强度
|
|
|
ASTM D-790
|
(-30°)
|
1300
|
kgf/cm
|
|
(80°)
|
260
|
kgf/cm
|
|
屈服下的伸张强度 (-30°)
|
1100
|
kgf/cm
|
ASTM D-638
|
屈服下的延伸率 (23°)
|
8
|
%
|
ASTM D-638
|
弯曲弹性率 (80°)
|
4000
|
kgf.cm/cm
|
ASTM D-256
|
屈服下的伸张强度 (23°)
|
420
|
kgf/cm
|
ASTM D-638
|
硬度(洛氏.布氏) (23°)
|
85
|
|
ASTM D-785
|
1%变形下的压缩强度 (23°)
|
200
|
kgf/cm
|
ASTM D-695
|
屈服下的伸张强度
|
|
|
ASTM D-638
|
(-30°)
|
900
|
kgf/cm
|
|
(80°)
|
200
|
kgf/cm
|
|
硬度(洛氏.布氏) (23°)
|
55
|
|
ASTM D-785
|
抗冲击强度 (-30°)
|
4.5
|
kgf.cm/cm
|
ASTM D-256
|
断裂下的延伸率 (23°)
|
100
|
%
|
ASTM D-638
|
屈服下的伸张强度 (23°)
|
800
|
kgf/cm
|
ASTM D-638
|
断裂下的延伸率 (23°)
|
>200
|
%
|
ASTM D-638
|
弯曲弹性率
|
|
|
ASTM D-790
|
(-30°)
|
29000
|
kgf/cm
|
|
(23°)
|
28500
|
kgf/cm
|
|
弯曲强度 (23°)
|
1100
|
kgf/cm
|
ASTM D-790
|
抗冲击强度 (23°)
|
6.5
|
kgf.cm/cm
|
ASTM D-256
|
弯曲强度 (80°)
|
500
|
kgf/cm
|
ASTM D-790
|
屈服下的伸张强度 (80°)
|
320
|
kgf/cm
|
ASTM D-638
|
弯曲弹性率
|
|
|
ASTM D-790
|
(-30°)
|
30000
|
kgf/cm
|
|
(23°)
|
7700
|
kgf/cm
|
|
(80°)
|
7500
|
kgf/cm
|
|
硬度(洛氏.布氏) (23°)
|
85
|
|
ASTM D-785
|
电气性能
|
额定值
|
单位
|
测试方法
|
介电常数 (10HZ)
|
8.0
|
|
ASTM D-150
|
介电损耗 (10HZ)
|
0.02
|
|
ASTM D-150
|
体积电阻率
|
10
|
Ω.cm
|
ASTM D-257
|
介电常数 (60HZ)
|
9.0
|
|
ASTM D-150
|
IEC电路
|
600+
|
V
|
UL746
|
介电常数
|
|
|
ASTM D-150
|
(60HZ)
|
3.9
|
|
|
(10HZ)
|
3.5
|
|
|
介电损耗 (10HZ)
|
0.10
|
|
ASTM D-150
|
抗电弧强度
|
119
|
S
|
ASTM D-495
|
介电常数 (10HZ)
|
3.8
|
|
ASTM D-150
|
介电损耗 (10HZ)
|
0.02
|
|
ASTM D-150
|
绝缘耐力
|
20
|
KV/mm
|
ASTM D-149
|
介电损耗
|
|
|
ASTM D-150
|
(60HZ)
|
0.10
|
|
|
(10HZ)
|
0.12
|
|
|
介电常数 (10HZ)
|
4.5
|
|
ASTM D-150
|
介电损耗 (60HZ)
|
0.01
|
|
ASTM D-150
|
体积电阻率
|
10
|
Ω.cm
|
ASTM D-257
|
热性能
|
额定值
|
单位
|
测试方法
|
热变形温度 (18.6kgf/cm)
|
75
|
°C
|
ASTM D-648
|
熔点 (DSC)
|
215-225
|
°C
|
|
线性热膨胀系数
|
8
|
X的10-5cm/cm/°C
|
ASTM D-696
|
热变形温度 (4.6kgf/cm)
|
180
|
°C
|
ASTM D-648
|
燃烧率
|
V-2
|
|
UL94
|

...